- Test for low workability / drier mix
- Slump test is carried out in cyclinder
- Lowered glass plate to surface of slump
- Switched on vibrating table
- Record time taken ( in second ) for remoulding ( for concrete slump to take the shape of cylinder - when lower surface of the glass plate is fully covered with cement grout ) .